Introduction :-




. POINT DEFECTS

Point defects are localized disruptions in otherwise perfect atomic or ionic arrangements in crystal structure. These imperfection may be introduced by movement of atoms or ions.
i) Vacancy
This is the simplest point defect. In this system, an atom is missing from its regular atomic site. It formed during solidification as a result of atomic vibrations and during recovery as a result of local rearrangement of atoms. Vacancies are also introduced during plastic deformation.

ii) Interstitialcy or Self-interstitial
Self-interstitial defect in a solid is obtained when an atom in a crystal occupies an interstitial site between surrounding atoms in normal atom sites.

Impurities in Solid
A pure metal consisting of just only one type of atom is not possible; impurity or foreign atoms will always be present, and some will exist as crystalline point defects.
Solid Solution
The simplest type of alloy is that of the solid solution. A solid solution is a solid that consists of two or more elements atomically dispersed in a single-phase structure. Impurity point defects are found in two types of solid solutions, namely, i) interstitial and ii) substitutional.
In interstitial solid solution, impurity atoms fill the voids or interstices among the host atoms. For metallic materials that have relatively high atomic packing factors, these interstitial positions are relatively small. Consequently, the atomic diameter of an interstitial impurity must be substantially smaller than that of the host atoms.
In substitutional solid solution, solute or impurity atoms replace the host atoms. The crystal structure of the parent element or solvent is unchanged.
Schottky Imperfections – When two oppositely charged ions are missing from an ionic crystal, a cation-anion vacancy is created which is known as a Schottky imperfection.

Frenkel Imperfection – If a positive cation moves into an interstitial site in an ionic crystal, a cation vacancy is created in the normal ion site. This vacancy-interstitialcy pair is called Frenkel Imperfection.

2. LINE DEFECTS

Line imperfections or defects in crystalline solids are defects that cause lattice distortion centered around a line. The main two types of dislocations are edge dislocations and screw dislocation, a combination of these two gives the mixed dislocations.

Edge Dislocation
An Edge Dislocation is created in a crystal by the intersection of an extra half plane of atoms. The inverted ‘tee’ indicates a positive edge dislocation, whereas upright ‘tee’ indicates a negative edge dislocation. The edge dislocation has a region of compressive strain where the extra half of plan is present and region tensile strain below the extra half plane of atoms
ii) Screw Dislocation
The Screw Dislocation can be formed in a perfect crystal by applying upward and downward shear stresses to regions of a perfect crystal, which have been separated by a cutting plane.
iii) Mixed Dislocation
Most dislocations in crystal are of mixed type having the edge and the screw components with a transition region between them.
Burgers Vector
Burgers vector characterizes a dislocation line. It indicates whether the dislocation line is an edge, screw or mixed dislocation. The Burgers vector is determined by carrying out a conventional procedure by tracing out a Burgers circuit. Burger vector is perpendicular to the edge dislocation.

 3. SURFACE DEFECTS

i) External Surface – One of the most obvious boundaries is the external surface, along which the structure terminates. Surface atoms are not bonded to the maximum number of nearest neighbors and therefore in a higher energy state than the atoms at interior position. To reduce this energy, materials tend to minimize.
ii) Grain Boundary and Interface – In this defect boundary separates two small grains or crystals having different crystallographic orientation in polycrystalline materials. In metals, grain boundaries are created during solidification, It is a narrow region of about two to five atomic diameters in width. Atomic packing in grain boundaries is lower than within the grains because of the atomic mismatch.
iii) Twin Boundary – Twin  boundary is a mirror reflection  of the atomic arrangement on the other side. Twin boundaries occur in pairs, such that the orientation change introduced by one boundary is restored by the other. The region between twin boundaries is called the twined region. Twins which form during the process of re-crystallization are called annealing twins, Whereas, twins form during plastic deformation are called deformation twins, commonly observed in HCP and BCC crystals.
iv) Stacking Fault – Stackin Faults are also planar surface imperfections created by a fault in stacking sequence of atoms planed in crystals.
ABCABCABC
If A is missing the stacking sequence become ABCABCABC. It is called HCP stacking.
v) Bulk or Volume Defects – These include pores, cracks, foreign inclusion and other phases.